Sign In | Join Free | My udpf.com
China Dongguan Zhongli Instrument Technology Co., Ltd. logo
Dongguan Zhongli Instrument Technology Co., Ltd.
Zhongli instrument,makes your laboratory more professional.
Verified Supplier

9 Years

Home > Rubber Testing Machine >

DSC-100 Differential Scanning Calorimeter Differential Scanning Calorimetry

Dongguan Zhongli Instrument Technology Co., Ltd.
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

DSC-100 Differential Scanning Calorimeter Differential Scanning Calorimetry

Brand Name : ZL

Model Number : ZL-3047A

Certification : ISO

Place of Origin : China

MOQ : 1 set

Price : Negotiable

Payment Terms : T/T,L/C,Western Union

Supply Ability : 100 set per month

Delivery Time : 7-10 days

Packaging Details : ISO 11357 Plastics Differential Scanning Calorimetry DSC Differential Scanning Calorimeter will be Packaged in wooden case (fumigation free)

Name : DSC-100 Differential Scanning Calorimeter Differential Scanning Calorimetry

Model : ZL-3047A

Temperature Range : Room temperature~600℃/-40~600℃ / -170~600℃

Temperature Resolution : 0.01℃ or 0.001℃

Temperature Fluctuation : ±0.1℃ or ±0.001℃

Temperature Repeatability : ±0.1℃ or ±0.01℃

Heating Rate/ Cooling Rate : 0.1~100℃ /min or 0.1~100℃/min/0.1~40℃ /min

Customized : can be customized

Warranty period : 2 Years

Contact Now

DSC-100 Differential Scanning Calorimeter
The DSC-100 Differential Scanning Calorimeter is a precision instrument designed for thermal analysis of materials. This heat flow type differential scanning calorimeter offers excellent repeatability and high accuracy, making it particularly suitable for specific heat measurements.
Instrument Overview
Differential Scanning Calorimetry (DSC) is widely used as both a routine quality testing tool and research instrument. The DSC-100 measures temperature and heat flow associated with thermal transitions within materials, providing critical data for material characterization.
Key Applications
  • Glass transition temperature measurement of polymer materials
  • Cold crystallization and phase transition analysis
  • Melting and crystallization behavior studies
  • Product stability and shelf-life assessment
  • Curing and crosslinking reaction monitoring
  • Oxidation induction period determination
  • Polymer material curing reaction temperature and thermal effect measurement
Measurement Principle
Samples and reference materials are placed in separate crucibles within the furnace and subjected to programmed heating. When sample and reference heat capacities are identical and no thermal effects occur, the temperature difference remains near zero, producing a smooth baseline curve. Thermal effects in the sample create temperature differences, with upward peaks indicating exothermic reactions and downward peaks representing endothermic processes.
Technical Specifications
Parameter ZL-DSC100A ZL-DSC300 ZL-DSC300C ZL-DSC300L
Temperature Range Room temperature~600℃ -40~600℃ -170~600℃ -170~600℃
Temperature Resolution 0.01℃ 0.001℃ 0.001℃ 0.001℃
Temperature Fluctuation ±0.1℃ ±0.001℃ ±0.01℃ ±0.01℃
Temperature Repeatability ±0.1℃ ±0.01℃ ±0.01℃ ±0.01℃
Heating/Cooling Rate 0.1~100℃/min 0.1~100℃/min 0.1~100℃/min 0.1~40℃/min
DSC Range 0~±600mW 0~±800mW 0~±600mW 0~±600mW
General Specifications
  • DSC Accuracy: 0.01mW
  • Power Supply: AC220V/50Hz or customized
  • Gas Flow Rate: 0~200mL/min
  • Gas Pressure: ≤0.5mPa
  • Display: 24-bit color, 7-inch LCD touch screen
  • Data Interface: Standard USB interface
DSC-100 Differential Scanning Calorimeter Differential Scanning Calorimetry

Product Tags:

DSC-100 differential scanning calorimeter

      

differential scanning calorimetry machine

      

rubber testing calorimeter with warranty

      
Best DSC-100 Differential Scanning Calorimeter Differential Scanning Calorimetry wholesale

DSC-100 Differential Scanning Calorimeter Differential Scanning Calorimetry Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Dongguan Zhongli Instrument Technology Co., Ltd.
*Subject:
*Message:
Characters Remaining: (0/3000)